COMSOL CD

SABIC Innovative Plastics CYCOLOY C1204HF ABS + Polycarbonate (North America)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: ABS Polymer; Polycarbonate; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesOriginal ValueComments
Density1.15 g/cc ASTM D 792
Density1.15 g/cc ISO 1183
Linear Mold Shrinkage0.005 - 0.007 cm/cm Flow, 0.125 inch; ASTM D 955
Melt Flow19 g/10 min 260C/5.0 kgf; ASTM D 1238
Melt Flow22 g/10 min Melt Volume Rate, MVR at 260C/5.0 kg; cm3/10min; ISO 1133
Melt Flow8 g/10 min Melt Volume Rate, MVR at 260C/2.16 kg; cm3/10min; ISO 1133

Mechanical Properties
Hardness, Rockwell R115 ISO 2039/2
Tensile Strength, Ultimate45 MPa 5 mm/min; ISO 527
Tensile Strength, Yield55 MPa 5 mm/min; ISO 527
Tensile Strength @ Yield8300 psi Type I, 2.0 in/min; ASTM D 638
Elongation at Break100 % 5 mm/min; ISO 527
Elongation at Break150 % Type I, 2.0 in/min; ASTM D 638
Elongation at Yield5 % Type I, 2.0 in/min; ASTM D 638
Elongation at Yield5 % 5 mm/min; ISO 527
Tensile Modulus2.4 GPa 1 mm/min; ISO 527
Tensile Modulus330000 psi 2.0 in/min; ASTM D 638
Flexural Modulus2.3 GPa 2 mm/min; ISO 178
Flexural Modulus340000 psi 0.05 in/min, 2" span; ASTM D 790
Flexural Yield Strength80 MPa 2 mm/min; ISO 178
Flexural Yield Strength12800 psi 0.05 in/min, 2" span; ASTM D 790
Izod Impact, Notched (ISO)41 kJ/m² 80*10*4 +23 C; ISO 180/ 1A
Izod Impact, Unnotched (ISO)NB 80*10*4 +23 C; ISO 180/ 1U
Izod Impact, Unnotched Low Temp (ISO)NB 80*10*4 -30 C; ISO 180/ 1U
Izod Impact, Notched, Low Temp (ISO)18 kJ/m² 80*10*4; -30 C; ISO 180/ 1A
Izod Impact, Notched, Low Temp9 ft-lb/in at -22F; ASTM D 256
Charpy Impact, Notched, Low Temp1.8 J/cm² at -30C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA
Charpy Impact, Notched4.5 J/cm² 23C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA
Gardner Impact @ 23°C480 in-lb Instrumented Impact Total Energy, 73°F; ASTM D 3763
Gardner Impact @ 23°C480 in-lb Instrumented Impact Total Energy, -22F; ASTM D 3763
Izod Impact, Notched11 ft-lb/in 73F; ASTM D 256

Electrical Properties
Volume ResistivityMin 1e+015 ohm-cm IEC 60093
Surface Resistivity per SquareMin 1e+015 ohm IEC 60093
Dielectric Constant2.7 1 MHz; IEC 60250
Dielectric Constant2.8 50 Hz; IEC 60250
Dielectric Strength17 kV/mm in oil, 3.2 mm; IEC 60243-1
Dielectric Strength25 kV/mm in oil, 1.6 mm; IEC 60243-1
Dielectric Strength35 kV/mm in oil, 0.8 mm; IEC 60243-1
Dissipation Factor0.002 50 Hz; IEC 60250
Dissipation Factor0.007 1 MHz; IEC 60250
Comparative Tracking Index250 - 400 V (+/- 0.125 inch); PLC Code 2; UL 746A
Hot Wire Ignition, HWI15 - 30 sec (+/- 0.125 inch); PLC Code 3; UL 746A
High Amp Arc Ignition, HAI60 - 120 arcs Surface (+/- 0.125 inch); PLC Code 1; UL 746A

Thermal Properties
CTE, linear 20°C80 µm/m-°C Flow 23C-60C; ISO 11359-2
CTE, linear 68°F40 µin/in-°F Flow, -40F to 100F; ASTM E 831
CTE, linear 20°C Transverse to Flow80 µm/m-°C 23C-60C; ISO 11359-2
Thermal Conductivity0.2 W/m-K ISO 8302
Deflection Temperature at 0.46 MPa (66 psi)122 °C HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 0.46 MPa (66 psi)259 °F 0.125 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)102 °C HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Deflection Temperature at 1.8 MPa (264 psi)229 °F 0.125 inch, unannealed; ASTM D 648
Vicat Softening Point126 °C B/50; ISO 306
Vicat Softening Point128 °C B/120; ISO 306
UL RTI, Electrical105 °C UL 746B
UL RTI, Mechanical with Impact80 °C UL 746B
UL RTI, Mechanical without Impact105 °C UL 746B
Flammability, UL94HB 0.047 in.
Oxygen Index23 % ISO 4589

Descriptive Properties
Ball Pressure Test, 125 C +/- 2 CPASSES IEC 60035-1
CSA File No.LS88480 
Hardness, H358/30 (MPa)96 ISO 2039/1
UL File Number, GLOBALE161759 
Printer friendly version Printer friendly version


New MatWeb Services

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。