SABIC Innovative Plastics CYCOLOY C2801 ABS + Polycarbonate (North America)
Subcategory: ABS Polymer; Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.
| Physical Properties | Original Value | Comments |
|
| Density | 1.22 g/cc | ASTM D 792 |
| Linear Mold Shrinkage | 0.004 - 0.005 cm/cm | Flow, 0.125 inch; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.003 - 0.005 cm/cm | 0.125 inch; ASTM D 955 |
Mechanical Properties |
|
| Tensile Strength @ Break | 7500 psi | Type I, 2.0 in/min; ASTM D 638 |
| Tensile Strength @ Yield | 9000 psi | Type I, 2.0 in/min; ASTM D 638 |
| Elongation at Break | 110 % | Type I, 2.0 in/min; ASTM D 638 |
| Flexural Modulus | 395000 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Flexural Yield Strength | 13800 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Coefficient of Friction | 0.21 | Vs. Steel, Kinetic; ASTM D 1894 |
| Coefficient of Friction, Static | 0.16 | Vs. Steel; ASTM D 1894 |
| K (wear) Factor | 430 x 10-10 in³-min/ft-lb-hr | PV = 2000 psi-fpm vs Steel; GE Test |
| Izod Impact, Notched | 2.5 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
| Comparative Tracking Index | 400 - 600 V | (+/- 0.125 inch); PLC Code 1; UL 746A |
| Hot Wire Ignition, HWI | 15 - 30 sec | (+/- 0.125 inch); PLC Code 3; UL 746A |
| High Amp Arc Ignition, HAI | Min 120 arcs | Surface (+/- 0.125 inch); PLC Code 0; UL 746A |
Thermal Properties |
|
| Deflection Temperature at 1.8 MPa (264 psi) | 180 °F | 0.250 inch, unannealed; ASTM D 648 |
| UL RTI, Electrical | 60 °C | UL 746B |
| UL RTI, Mechanical with Impact | 60 °C | UL 746B |
| UL RTI, Mechanical without Impact | 60 °C | UL 746B |
| Flammability, UL94 | V-0 | 0.059 in. |
| Flammability, UL94 | 6 | 0.098 in. |
Descriptive Properties | |
| UL File Number, USA | E121562 | |
|
Printer friendly version |
|