SABIC Innovative Plastics CYCOLOY C6200 ABS + Polycarbonate (North America)
Subcategory: ABS Polymer; Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.
| Physical Properties | Original Value | Comments |
|
| Density | 1.18 g/cc | ASTM D 792 |
| Linear Mold Shrinkage | 0.004 - 0.006 cm/cm | Flow, 0.125 inch; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.004 - 0.006 cm/cm | 0.125 inch; ASTM D 955 |
| Melt Flow | 14.5 g/10 min | 260C/2.16 kgf; ASTM D 1238 |
| Spiral Flow | 27 in | 500F, 10 ips, .125 X 60 in |
Mechanical Properties |
|
| Tensile Strength @ Yield | 9700 psi | Type I, 2.0 in/min; ASTM D 638 |
| Elongation at Break | 50 % | Type I, 2.0 in/min; ASTM D 638 |
| Flexural Modulus | 390000 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Flexural Yield Strength | 15000 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Gardner Impact @ 23°C | 480 in-lb | Instrumented Impact Energy @ peak, -22°F; ASTM D 3763 |
| Gardner Impact @ 23°C | 540 in-lb | Instrumented Impact Energy @ peak, 73F; ASTM D 3763 |
| Izod Impact, Notched | 10 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
| Volume Resistivity | Min 1e+015 ohm-cm | IEC 60093 |
| Surface Resistivity per Square | Min 1e+015 ohm | IEC 60093 |
| Dielectric Constant | 2.7 | 1 MHz; IEC 60250 |
| Dielectric Constant | 2.8 | 50 Hz; IEC 60250 |
| Dielectric Strength | 17 kV/mm | in oil, 3.2 mm; IEC 60243-1 |
| Dielectric Strength | 25 kV/mm | in oil, 1.6 mm; IEC 60243-1 |
| Dielectric Strength | 35 kV/mm | in oil, 0.8 mm; IEC 60243-1 |
| Dissipation Factor | 0.004 | 50 Hz; IEC 60250 |
| Dissipation Factor | 0.008 | 1 MHz; IEC 60250 |
| Arc Resistance | 60 - 120 sec | Tungsten (+/- 0.125 inch); PLC Code 6; ASTM D 495 |
| Comparative Tracking Index | 250 - 400 V | (+/- 0.125 inch); PLC Code 2; UL 746A |
| Hot Wire Ignition, HWI | 30 - 60 sec | (+/- 0.125 inch); PLC Code 2; UL 746A |
| High Amp Arc Ignition, HAI | Min 120 arcs | Surface (+/- 0.125 inch); PLC Code 0; UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | 80 - 150 mm/min | (+/- 0.125 inch); PLC Code 3; UL 746A |
Thermal Properties |
|
| Deflection Temperature at 1.8 MPa (264 psi) | 190 °F | 0.125 inch, unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °F | 0.250 inch, unannealed; ASTM D 648 |
| UL RTI, Electrical | 85 °C | UL 746B |
| UL RTI, Mechanical with Impact | 85 °C | UL 746B |
| UL RTI, Mechanical without Impact | 85 °C | UL 746B |
| Flammability, UL94 | HB | 0.028 in. |
| Flammability, UL94 | V-1 | 0.048 in. |
| Flammability, UL94 | V-0 | 0.058 in. |
| Flammability, UL94 | 6 | 0.079 in. |
| Flammability, UL94 | 7 | 0.134 in. |
Descriptive Properties | |
| CSA File No. | LS88480 | |
| UL File Number, GLOBAL | E161759 | |
| UL File Number, USA | E121562 | |
|