Physical Properties | Original Value | Comments |
|
Density | 1.19 g/cc | ASTM D 792 |
Water Absorption | 0.11 % | 24 hours @ 73F; ASTM D 570 |
Linear Mold Shrinkage | 0.004 - 0.006 cm/cm | Flow, 0.125 inch; ASTM D 955 |
Melt Flow | 21.5 g/10 min | 260C/2.16 kgf; ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Break | 7100 psi | Type I, 2.0 in/min; ASTM D 638 |
Tensile Strength @ Yield | 9200 psi | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Break | 80 % | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Yield | 4 % | Type I, 2.0 in/min; ASTM D 638 |
Tensile Modulus | 435000 psi | 2.0 in/min; ASTM D 638 |
Flexural Modulus | 380000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Yield Strength | 13700 psi | 0.05 in/min, 2" span; ASTM D 790 |
Gardner Impact @ 23°C | 450 in-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
Gardner Impact @ 23°C | 450 in-lb | Instrumented Impact Total Energy, -22F; ASTM D 3763 |
Izod Impact, Notched | 11 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
Volume Resistivity | Min 1e+015 ohm-cm | IEC 60093 |
Surface Resistivity per Square | Min 1e+015 ohm | IEC 60093 |
Dielectric Constant | 2.7 | 50 Hz; IEC 60250 |
Dielectric Constant | 2.7 | 1 MHz; IEC 60250 |
Dielectric Strength | 17 kV/mm | in oil, 3.2 mm; IEC 60243-1 |
Dissipation Factor | 0.004 | 50 Hz; IEC 60250 |
Dissipation Factor | 0.006 | 1 MHz; IEC 60250 |
Comparative Tracking Index | 600 V | IEC 112/3rd |
Thermal Properties |
|
Deflection Temperature at 0.46 MPa (66 psi) | 208 °F | 0.125 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 194 °F | 0.125 inch, unannealed; ASTM D 648 |
Vicat Softening Point | 211 °F | Rate B; ASTM D 1525 |
UL RTI, Electrical | 80 °C | UL 746B |
UL RTI, Mechanical with Impact | 70 °C | UL 746B |
UL RTI, Mechanical without Impact | 80 °C | UL 746B |
Flammability, UL94 | V-2 | 0.03 in. |
Flammability, UL94 | V-0 | 0.059 in. |
Flammability, UL94 | 6 | 0.079 in. |
Descriptive Properties | |
UL File Number, GLOBAL | E161759 | |
UL File Number, USA | E121562 | |
|