SABIC Innovative Plastics CYCOLOY C7210A ABS + Polycarbonate (North America)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: ABS Polymer; Polycarbonate; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line.

Physical PropertiesOriginal ValueComments
Density1.22 g/cc ASTM D 792
Linear Mold Shrinkage0.003 - 0.005 cm/cm Flow, 0.125 inch; ASTM D 955
Linear Mold Shrinkage, Transverse0.004 - 0.006 cm/cm 0.125 inch; ASTM D 955
Melt Flow16.4 g/10 min 260C/2.16 kgf; ASTM D 1238

Mechanical Properties
Tensile Strength @ Break7100 psi Type I, 0.2 in/min; ASTM D 638
Tensile Strength @ Yield9200 psi Type I, 0.2 in/min; ASTM D 638
Elongation at Break80 % Type I, 0.2 in/min; ASTM D 638
Elongation at Yield3.6 % Type I, 0.2 in/min; ASTM D 638
Tensile Modulus510000 psi 0.2 in/min; ASTM D 638
Flexural Modulus456000 psi 0.05 in/min, 2" span; ASTM D 790
Flexural Strength15400 psi 0.05 in/min, 2" span; ASTM D 790
Izod Impact, Unnotched35 ft-lb/in 73F; ASTM D 4812
Gardner Impact @ 23°C420 in-lb Instrumented Impact Total Energy, 73°F; ASTM D 3763
Izod Impact, Notched3.3 ft-lb/in 73F; ASTM D 256

Thermal Properties
CTE, linear 68°F33 µin/in-°F Flow, -40F to 100F; ASTM E 831
CTE, linear 68°F, Transverse to Flow37 µin/in-°F from -40F to 100F; ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi)198 °F 0.125 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)180 °F 0.125 inch, unannealed; ASTM D 648
Vicat Softening Point215 °F Rate B; ASTM D 1525
UL RTI, Electrical60 °C UL 746B
UL RTI, Mechanical with Impact60 °C UL 746B
UL RTI, Mechanical without Impact60 °C UL 746B
Flammability, UL94V-0 0.047 in.
Flammability, UL946 0.078 in.

Descriptive Properties
UL File Number, GLOBALE161759 
UL File Number, USAE121562 
Printer friendly version Printer friendly version


Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。