MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

COMSOL CD

SABIC Innovative Plastics CYCOLOY FXC810AR ABS + Polycarbonate (North America)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: ABS Polymer; Polycarbonate; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesOriginal ValueComments
Density1.18 g/cc ASTM D 792
Linear Mold Shrinkage0.004 - 0.006 cm/cm Flow, 0.125 inch; ASTM D 955
Melt Flow22 g/10 min 260C/5.0 kgf; ASTM D 1238

Mechanical Properties
Tensile Strength @ Break6500 psi Type I, 2.0 in/min; ASTM D 638
Tensile Strength @ Yield7500 psi Type I, 2.0 in/min; ASTM D 638
Elongation at Break50 % Type I, 2.0 in/min; ASTM D 638
Elongation at Yield5 % Type I, 2.0 in/min; ASTM D 638
Tensile Modulus360000 psi 2.0 in/min; ASTM D 638
Flexural Modulus350000 psi 0.05 in/min, 2" span; ASTM D 790
Flexural Yield Strength11000 psi 0.05 in/min, 2" span; ASTM D 790
Gardner Impact @ 23°C360 in-lb Instrumented Impact Total Energy, 73°F; ASTM D 3763
Izod Impact, Notched8 ft-lb/in 73F; ASTM D 256

Thermal Properties
CTE, linear 68°F40 µin/in-°F Flow, -40F to 100F; ASTM E 831
CTE, linear 68°F, Transverse to Flow40 µin/in-°F from -40F to 100F; ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi)268 °F 0.125 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)235 °F 0.125 inch, unannealed; ASTM D 648
Vicat Softening Point290 °F Rate B; ASTM D 1525
Printer friendly version Printer friendly version


New MatWeb Services

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。