SABIC Innovative Plastics CYCOLOY LG8002 ABS + Polycarbonate (North America)
Subcategory: ABS Polymer; Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
Physical Properties | Original Value | Comments |
|
Density | 1.13 g/cc | ASTM D 792 |
Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | Flow, 0.125 inch; ASTM D 955 |
Melt Flow | 6.5 g/10 min | 260C/5.0 kgf; ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Yield | 8100 psi | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Break | 120 % | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Yield | 5 % | Type I, 2.0 in/min; ASTM D 638 |
Flexural Modulus | 330000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Yield Strength | 12400 psi | 0.05 in/min, 2" span; ASTM D 790 |
Izod Impact, Notched, Low Temp | 11 ft-lb/in | at -22F; ASTM D 256 |
Gardner Impact @ 23°C | 360 in-lb | Instrumented Impact Total Energy, -22F; ASTM D 3763 |
Gardner Impact @ 23°C | 420 in-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
Izod Impact, Notched | 12 ft-lb/in | 73F; ASTM D 256 |
Thermal Properties |
|
CTE, linear 68°F | 50 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
Thermal Conductivity | 0.25 W/m-K | ASTM C 177 |
Deflection Temperature at 0.46 MPa (66 psi) | 250 °F | 0.125 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 220 °F | 0.125 inch, unannealed; ASTM D 648 |
Optical Properties |
|
Gloss | 30 % | Untextured, 60 degrees; ASTM D 523 |
|