Physical Properties | Original Value | Comments |
|
Density | 1.1 g/cc | ASTM D 792 |
Water Absorption | 0.1 % | 24 hours @ 73F; ASTM D 570 |
Linear Mold Shrinkage | 0.005 - 0.008 cm/cm | Flow, 0.125 inch; ASTM D 955 |
Linear Mold Shrinkage, Transverse | 0.005 - 0.007 cm/cm | 0.125 inch; ASTM D 955 |
Melt Flow | 14 g/10 min | 260C/5.0 kgf; ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Break | 6400 psi | Type I, 2.0 in/min; ASTM D 638 |
Tensile Strength @ Yield | 7300 psi | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Break | 150 % | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Yield | 8.6 % | Type I, 2.0 in/min; ASTM D 638 |
Tensile Modulus | 310000 psi | 2.0 in/min; ASTM D 638 |
Flexural Modulus | 300000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Yield Strength | 10500 psi | 0.05 in/min, 2" span; ASTM D 790 |
Izod Impact, Notched, Low Temp | 8 ft-lb/in | at -22F; ASTM D 256 |
Gardner Impact @ 23°C | 300 in-lb | Instrumented Impact Total Energy, -22F; ASTM D 3763 |
Gardner Impact @ 23°C | 360 in-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
Izod Impact, Notched | 10 ft-lb/in | 73F; ASTM D 256 |
Thermal Properties |
|
CTE, linear 68°F | 40 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
CTE, linear 68°F, Transverse to Flow | 50 µin/in-°F | from -40F to 100F; ASTM E 831 |
Thermal Conductivity | 0.2 W/m-K | ASTM C 177 |
Deflection Temperature at 0.46 MPa (66 psi) | 240 °F | 0.125 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 210 °F | 0.125 inch, unannealed; ASTM D 648 |
Vicat Softening Point | 233 °F | Rate B; ASTM D 1525 |
|