SABIC Innovative Plastics CYCOLOY MC7000 ABS + Polycarbonate (North America)
Subcategory: ABS Polymer; Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
| Physical Properties | Original Value | Comments |
|
| Density | 1.11 g/cc | ASTM D 792 |
| Linear Mold Shrinkage | 0.005 - 0.008 cm/cm | Flow, 0.125 inch; ASTM D 955 |
| Melt Flow | 13 g/10 min | 260C/5.0 kgf; ASTM D 1238 |
Mechanical Properties |
|
| Tensile Strength @ Yield | 8100 psi | Type I, 2.0 in/min; ASTM D 638 |
| Elongation at Break | 145 % | Type I, 2.0 in/min; ASTM D 638 |
| Tensile Modulus | 350000 psi | 2.0 in/min; ASTM D 638 |
| Flexural Modulus | 330000 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Flexural Yield Strength | 11900 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Izod Impact, Notched, Low Temp | 9 ft-lb/in | at -22F; ASTM D 256 |
| Gardner Impact @ 23°C | 480 in-lb | Instrumented Impact Total Energy, -22F; ASTM D 3763 |
| Gardner Impact @ 23°C | 540 in-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
| Izod Impact, Notched | 11 ft-lb/in | 73F; ASTM D 256 |
Thermal Properties |
|
| CTE, linear 68°F | 40 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
| Deflection Temperature at 1.8 MPa (264 psi) | 212 °F | 0.250 inch, unannealed; ASTM D 648 |
|