SABIC Innovative Plastics CYCOLOY MC8002 ABS + Polycarbonate (North America)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: ABS Polymer; Polycarbonate; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line.

Physical PropertiesOriginal ValueComments
Density1.14 g/cc ASTM D 792
Water Absorption0.1 % 24 hours @ 73F; ASTM D 570
Water Absorption at Saturation0.4 % Equilibrium, 73F; ASTM D 570
Linear Mold Shrinkage0.005 - 0.007 cm/cm Flow, 0.125 inch; ASTM D 955
Melt Flow9 g/10 min 260C/5.0 kgf; ASTM D 1238

Mechanical Properties
Tensile Strength @ Yield8200 psi Type I, 2.0 in/min; ASTM D 638
Elongation at Break150 % Type I, 2.0 in/min; ASTM D 638
Elongation at Yield5 % Type I, 2.0 in/min; ASTM D 638
Tensile Modulus320000 psi 2.0 in/min; ASTM D 638
Flexural Modulus340000 psi 0.05 in/min, 2" span; ASTM D 790
Flexural Yield Strength12500 psi 0.05 in/min, 2" span; ASTM D 790
Izod Impact, Notched, Low Temp10 ft-lb/in at -22F; ASTM D 256
Gardner Impact @ 23°C480 in-lb Instrumented Impact Total Energy, -22F; ASTM D 3763
Gardner Impact @ 23°C540 in-lb Instrumented Impact Total Energy, 73°F; ASTM D 3763
Izod Impact, Notched12 ft-lb/in 73F; ASTM D 256

Thermal Properties
CTE, linear 68°F40 µin/in-°F Flow, -40F to 100F; ASTM E 831
Thermal Conductivity0.2 W/m-K ASTM C 177
Deflection Temperature at 0.46 MPa (66 psi)255 °F 0.125 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)225 °F 0.125 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)230 °F 0.250 inch, unannealed; ASTM D 648
Printer friendly version Printer friendly version


Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。