SABIC Innovative Plastics ULTEM ATX100R Polyetherimide (North America)
Subcategory: Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
| Physical Properties | Original Value | Comments |
|
| Density | 1.21 g/cc | ASTM D 792 |
| Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | Flow, 0.125 inch; ASTM D 955 |
| Melt Flow | 6.4 g/10 min | 295C/6.6 kgf; ASTM D 1238 |
Mechanical Properties |
|
| Tensile Strength @ Yield | 10000 psi | Type I, 0.2 in/min; ASTM D 638 |
| Elongation at Break | 80 % | Type I, 0.2 in/min; ASTM D 638 |
| Flexural Modulus | 368000 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Flexural Yield Strength | 15500 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Izod Impact, Unnotched | 39 ft-lb/in | 73F; ASTM D 4812 |
| Izod Impact, Notched | 7 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
| Comparative Tracking Index | 175 - 250 V | (+/- 0.125 inch); PLC Code 3; UL 746A |
| Hot Wire Ignition, HWI | 60 - 120 sec | (+/- 0.125 inch); PLC Code 1; UL 746A |
| High Amp Arc Ignition, HAI | Min 120 arcs | Surface (+/- 0.125 inch); PLC Code 0; UL 746A |
Thermal Properties |
|
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °F | 0.250 inch, unannealed; ASTM D 648 |
| UL RTI, Electrical | 115 °C | UL 746B |
| UL RTI, Mechanical with Impact | 115 °C | UL 746B |
| UL RTI, Mechanical without Impact | 115 °C | UL 746B |
| Flammability, UL94 | HB | 0.03 in. |
Descriptive Properties | |
| UL File Number, USA | E121562 | |
|