SABIC Innovative Plastics ULTEM LTX300B Polyetherimide (North America)
Subcategory: Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.27 g/cc | ASTM D 792 |
Halogen Content | 0 % | GE Test |
Linear Mold Shrinkage | 0.003 - 0.005 cm/cm | Flow, 0.125 inch; ASTM D 955 |
Linear Mold Shrinkage, Transverse | 0.005 - 0.007 cm/cm | 0.125 inch; ASTM D 955 |
Melt Flow | 1.6 g/10 min | 295C/6.6 kgf; ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Yield | 14000 psi | Type I, 0.2 in/min; ASTM D 638 |
Elongation at Break | 88 % | Type I, 0.2 in/min; ASTM D 638 |
Tensile Modulus | 485000 psi | 0.2 in/min; ASTM D 638 |
Flexural Modulus | 465000 psi | 0.10 in/min, 4" span; ASTM D 790 |
Flexural Strength | 20500 psi | 0.10 in/min, 4" span; ASTM D 790 |
Flexural Yield Strength | 21000 psi | 0.10 in/min, 4" span; ASTM D 790 |
Gardner Impact | 26 ft-lb | 73F; ASTM D 3029 |
Izod Impact, Notched | 1.5 ft-lb/in | 73F; ASTM D 256 |
Izod Impact, Notched | 40 ft-lb/in | Reverse Notched, 73F; ASTM D 256 |
Electrical Properties |
|
Arc Resistance | 60 - 120 sec | Tungsten (+/- 0.125 inch); PLC Code 6; ASTM D 495 |
Comparative Tracking Index | 100 - 175 V | (+/- 0.125 inch); PLC Code 4; UL 746A |
Hot Wire Ignition, HWI | Min 120 sec | (+/- 0.125 inch); PLC Code 0; UL 746A |
High Amp Arc Ignition, HAI | Min 120 arcs | Surface (+/- 0.125 inch); PLC Code 0; UL 746A |
High Voltage Arc-Tracking Rate, HVTR | 80 - 150 mm/min | (+/- 0.125 inch); PLC Code 3; UL 746A |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 375 °F | 0.250 inch, unannealed; ASTM D 648 |
UL RTI, Electrical | 140 °C | UL 746B |
UL RTI, Mechanical with Impact | 115 °C | UL 746B |
UL RTI, Mechanical without Impact | 140 °C | UL 746B |
Flammability, UL94 | V-0 | 0.03 in. |
Descriptive Properties | |
UL File Number, USA | E121562 | |
|