Physical Properties | Original Value | Comments |
|
Density | 1.27 g/cc | ASTM D 792 |
Water Absorption | 0.25 % | 24 hours @ 73F; ASTM D 570 |
Water Absorption at Saturation | 1.25 % | Equilibrium, 73F; ASTM D 570 |
Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | Flow, 0.125 inch; ASTM D 955 |
Melt Flow | 12 g/10 min | 337C/6.6 kgf; ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Yield | 16000 psi | Type I, 0.2 in/min; ASTM D 638 |
Elongation at Break | 60 % | Type I, 0.2 in/min; ASTM D 638 |
Elongation at Yield | 7 % | Type I, 0.2 in/min; ASTM D 638 |
Tensile Modulus | 520000 psi | 0.2 in/min; ASTM D 638 |
Flexural Modulus | 510000 psi | 0.10 in/min, 4" span; ASTM D 790 |
Flexural Yield Strength | 24000 psi | 0.10 in/min, 4" span; ASTM D 790 |
Poisson's Ratio | 0.36 | ASTM D 638 |
Izod Impact, Unnotched | 25 ft-lb/in | 73F; ASTM D 4812 |
Izod Impact, Notched | 1 ft-lb/in | 73F; ASTM D 256 |
Thermal Properties |
|
CTE, linear, 212°F (100°C) | 30 µin/in-°F | Cross Flow; 0F to 300F; ASTM E 831 |
CTE, linear, 212°F (100°C) | 31 µin/in-°F | Flow, 0F to 300F; ASTM E 831 |
Thermal Conductivity | 0.22 W/m-K | ASTM C 177 |
Deflection Temperature at 0.46 MPa (66 psi) | 410 °F | 0.250 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 394 °F | 0.250 inch, unannealed; ASTM D 648 |
Vicat Softening Point | 426 °F | Rate B; ASTM D 1525 |
|