MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

COMSOL CD

SABIC Innovative Plastics ULTEM 1000R Polyetherimide (North America)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.

Physical PropertiesOriginal ValueComments
Density1.27 g/cc ASTM D 792
Water Absorption0.25 % 24 hours @ 73F; ASTM D 570
Water Absorption at Saturation1.25 % Equilibrium, 73F; ASTM D 570
Linear Mold Shrinkage0.005 - 0.007 cm/cm Flow, 0.125 inch; ASTM D 955
Melt Flow9.7 g/10 min 337C/6.6 kgf; ASTM D 1238

Mechanical Properties
Hardness, Rockwell M109 ASTM D 785
Tensile Strength @ Yield16000 psi Type I, 0.2 in/min; ASTM D 638
Elongation at Break60 % Type I, 0.2 in/min; ASTM D 638
Elongation at Yield7 % Type I, 0.2 in/min; ASTM D 638
Tensile Modulus520000 psi 0.2 in/min; ASTM D 638
Flexural Modulus510000 psi 0.10 in/min, 4" span; ASTM D 790
Flexural Yield Strength24000 psi 0.10 in/min, 4" span; ASTM D 790
Poisson's Ratio0.36 ASTM D 638
Izod Impact, Unnotched25 ft-lb/in 73F; ASTM D 4812
Gardner Impact27 ft-lb 73F; ASTM D 3029
Taber Abrasion, mg/1000 Cycles10 CS-17, 1 kg; ASTM D 1044
Izod Impact, Notched1 ft-lb/in 73F; ASTM D 256
Izod Impact, Notched30 ft-lb/in Reverse Notched, 73F; ASTM D 256

Electrical Properties
Volume Resistivity1e+017 ohm-cm ASTM D 257
Dielectric Constant3.15 1 kHz; ASTM D 150
Dielectric Strength710 V/mil in oil, 62 mils; ASTM D 149
Dielectric Strength831 V/mil in air, 62 mils; ASTM D 149
Dissipation Factor0.0013 1 kHz; ASTM D 150
Dissipation Factor0.0025 2450 MHz; ASTM D 150
Arc Resistance120 - 180 sec Tungsten (+/- 0.125 inch); PLC Code 5; ASTM D 495
Comparative Tracking Index100 - 175 V (+/- 0.125 inch); PLC Code 4; UL 746A
Hot Wire Ignition, HWI60 - 120 sec (+/- 0.125 inch); PLC Code 1; UL 746A
High Amp Arc Ignition, HAI15 - 30 arcs Surface (+/- 0.125 inch); PLC Code 3; UL 746A
High Voltage Arc-Tracking Rate, HVTR25.4 - 80 mm/min (+/- 0.125 inch); PLC Code 2; UL 746A

Thermal Properties
CTE, linear, 212°F (100°C)30 µin/in-°F Cross Flow; 0F to 300F; ASTM E 831
CTE, linear, 212°F (100°C)31 µin/in-°F Flow, 0F to 300F; ASTM E 831
Thermal Conductivity0.22 W/m-K ASTM C 177
Deflection Temperature at 0.46 MPa (66 psi)410 °F 0.250 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)394 °F 0.250 inch, unannealed; ASTM D 648
Vicat Softening Point426 °F Rate B; ASTM D 1525
UL RTI, Electrical170 °C UL 746B
UL RTI, Mechanical with Impact170 °C UL 746B
UL RTI, Mechanical without Impact170 °C UL 746B
Flammability, UL94V-0 0.016 in.
Flammability, UL947 0.075 in.
NBS Smoke Density0.7 Flaming, Ds 4 min; ASTM E 662
NBS Smoke Density30 Flaming, Dmax 20 min; ASTM E 662
Oxygen Index47 % ASTM D 2863

Descriptive Properties
UL File Number, USAE121562 
Printer friendly version Printer friendly version


Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。