COMSOL CD

SABIC Innovative Plastics ULTEM 1110F Polyetherimide (North America)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesOriginal ValueComments
Density1.36 g/cc ASTM D 792
Linear Mold Shrinkage0.005 - 0.007 cm/cm Flow, 0.125 inch; ASTM D 955
Melt Flow16 g/10 min 337C/6.6 kgf; ASTM D 1238

Mechanical Properties
Tensile Strength @ Yield16000 psi Type I, 0.2 in/min; ASTM D 638
Elongation at Break70 % Type I, 0.2 in/min; ASTM D 638
Tensile Modulus540000 psi 0.2 in/min; ASTM D 638
Flexural Modulus540000 psi 0.10 in/min, 4" span; ASTM D 790
Flexural Yield Strength24000 psi 0.10 in/min, 4" span; ASTM D 790
Gardner Impact17 ft-lb 73F; ASTM D 3029
Izod Impact, Notched36 ft-lb/in Reverse Notched, 73F; ASTM D 256

Electrical Properties
Arc Resistance120 - 180 sec Tungsten (+/- 0.125 inch); PLC Code 5; ASTM D 495
Comparative Tracking Index100 - 175 V (+/- 0.125 inch); PLC Code 4; UL 746A
Hot Wire Ignition, HWI60 - 120 sec (+/- 0.125 inch); PLC Code 1; UL 746A
High Amp Arc Ignition, HAI15 - 30 arcs Surface (+/- 0.125 inch); PLC Code 3; UL 746A
High Voltage Arc-Tracking Rate, HVTR25.4 - 80 mm/min (+/- 0.125 inch); PLC Code 2; UL 746A

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)390 °F 0.250 inch, unannealed; ASTM D 648
UL RTI, Electrical170 °C UL 746B
UL RTI, Mechanical with Impact170 °C UL 746B
UL RTI, Mechanical without Impact170 °C UL 746B
Flammability, UL94V-2 0.028 in.
Flammability, UL94V-0 0.028 in.
Flammability, UL947 0.118 in.

Descriptive Properties
UL File Number, USAE121562 
Printer friendly version Printer friendly version


New MatWeb Services

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。