SABIC Innovative Plastics ULTEM 2212R Polyetherimide (North America)
Subcategory: Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.43 g/cc | ASTM D 792 |
Melt Flow | 13.5 g/10 min | 337C/6.6 kgf; ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Break | 13400 psi | Type I, 0.2 in/min; ASTM D 638 |
Elongation at Break | 6 % | Type I, 0.2 in/min; ASTM D 638 |
Tensile Modulus | 620000 psi | 0.2 in/min; ASTM D 638 |
Flexural Modulus | 740000 psi | 0.10 in/min, 4" span; ASTM D 790 |
Flexural Strength | 25000 psi | 0.10 in/min, 4" span; ASTM D 790 |
Izod Impact, Notched | 0.9 ft-lb/in | 73F; ASTM D 256 |
Izod Impact, Notched | 7.2 ft-lb/in | Reverse Notched, 73F; ASTM D 256 |
Electrical Properties |
|
Arc Resistance | Max 60 sec | Tungsten (+/- 0.125 inch); PLC Code 7; ASTM D 495 |
Comparative Tracking Index | 100 - 175 V | (+/- 0.125 inch); PLC Code 4; UL 746A |
Hot Wire Ignition, HWI | 60 - 120 sec | (+/- 0.125 inch); PLC Code 1; UL 746A |
High Amp Arc Ignition, HAI | 15 - 30 arcs | Surface (+/- 0.125 inch); PLC Code 3; UL 746A |
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80 mm/min | (+/- 0.125 inch); PLC Code 2; UL 746A |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 402 °F | 0.250 inch, unannealed; ASTM D 648 |
UL RTI, Electrical | 170 °C | UL 746B |
UL RTI, Mechanical with Impact | 170 °C | UL 746B |
UL RTI, Mechanical without Impact | 170 °C | UL 746B |
Flammability, UL94 | V-0 | 0.016 in. |
Descriptive Properties | |
UL File Number, USA | E121562 | |
|