| Physical Properties | Original Value | Comments |
|
| Density | 1.51 g/cc | ASTM D 792 |
| Linear Mold Shrinkage | 0.002 - 0.004 cm/cm | Flow, 0.125 inch; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.002 - 0.004 cm/cm | 0.125 inch; ASTM D 955 |
| Melt Flow | 7.6 g/10 min | 337C/6.6 kgf; ASTM D 1238 |
Mechanical Properties |
|
| Tensile Strength @ Break | 23000 psi | Type I, 0.2 in/min; ASTM D 638 |
| Tensile Strength @ Yield | 24500 psi | Type I, 0.2 in/min; ASTM D 638 |
| Elongation at Break | 2 % | Type I, 0.2 in/min; ASTM D 638 |
| Tensile Modulus | 1.34e+006 psi | 0.2 in/min; ASTM D 638 |
| Flexural Modulus | 1.34e+006 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Flexural Strength | 32000 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Izod Impact, Notched | 1.6 ft-lb/in | 73F; ASTM D 256 |
| Izod Impact, Notched | 8.2 ft-lb/in | Reverse Notched, 73F; ASTM D 256 |
Electrical Properties |
|
| Arc Resistance | 60 - 120 sec | Tungsten (+/- 0.125 inch); PLC Code 6; ASTM D 495 |
| Comparative Tracking Index | 100 - 175 V | (+/- 0.125 inch); PLC Code 4; UL 746A |
| Hot Wire Ignition, HWI | 60 - 120 sec | (+/- 0.125 inch); PLC Code 1; UL 746A |
| High Amp Arc Ignition, HAI | Max 15 arcs | Surface (+/- 0.125 inch); PLC Code 4; UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | 80 - 150 mm/min | (+/- 0.125 inch); PLC Code 3; UL 746A |
Thermal Properties |
|
| CTE, linear, 212°F (100°C) | 23 µin/in-°F | Cross Flow; 0F to 300F; ASTM E 831 |
| CTE, linear, 212°F (100°C) | 9 µin/in-°F | Flow, 0F to 300F; ASTM E 831 |
| Deflection Temperature at 1.8 MPa (264 psi) | 410 °F | 0.250 inch, unannealed; ASTM D 648 |
| UL RTI, Electrical | 180 °C | UL 746B |
| UL RTI, Mechanical with Impact | 170 °C | UL 746B |
| UL RTI, Mechanical without Impact | 180 °C | UL 746B |
| Flammability, UL94 | V-0 | 0.01 in. |
| Flammability, UL94 | 7 | 0.048 in. |
Descriptive Properties | |
| UL File Number, USA | E121562 | |
|