COMSOL CD

SABIC Innovative Plastics ULTEM 2310R Polyetherimide (North America)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesOriginal ValueComments
Density1.51 g/cc ASTM D 792
Melt Flow7.6 g/10 min 337C/6.6 kgf; ASTM D 1238

Mechanical Properties
Tensile Strength @ Break23000 psi Type I, 0.2 in/min; ASTM D 638
Tensile Strength @ Yield24500 psi Type I, 0.2 in/min; ASTM D 638
Elongation at Break2 % Type I, 0.2 in/min; ASTM D 638
Tensile Modulus1.34e+006 psi 0.2 in/min; ASTM D 638
Flexural Modulus1.34e+006 psi 0.10 in/min, 4" span; ASTM D 790
Flexural Strength32000 psi 0.10 in/min, 4" span; ASTM D 790
Izod Impact, Notched1.6 ft-lb/in 73F; ASTM D 256
Izod Impact, Notched9 ft-lb/in Reverse Notched, 73F; ASTM D 256

Electrical Properties
Arc Resistance60 - 120 sec Tungsten (+/- 0.125 inch); PLC Code 6; ASTM D 495
Comparative Tracking Index100 - 175 V (+/- 0.125 inch); PLC Code 4; UL 746A
Hot Wire Ignition, HWI60 - 120 sec (+/- 0.125 inch); PLC Code 1; UL 746A
High Amp Arc Ignition, HAIMax 15 arcs Surface (+/- 0.125 inch); PLC Code 4; UL 746A
High Voltage Arc-Tracking Rate, HVTR80 - 150 mm/min (+/- 0.125 inch); PLC Code 3; UL 746A

Thermal Properties
CTE, linear, 212°F (100°C)23 µin/in-°F Cross Flow; 0F to 300F; ASTM E 831
CTE, linear, 212°F (100°C)9 µin/in-°F Flow, 0F to 300F; ASTM E 831
Deflection Temperature at 1.8 MPa (264 psi)412 °F 0.250 inch, unannealed; ASTM D 648
UL RTI, Electrical180 °C UL 746B
UL RTI, Mechanical with Impact170 °C UL 746B
UL RTI, Mechanical without Impact180 °C UL 746B
Flammability, UL94V-0 0.01 in.
Flammability, UL947 0.048 in.

Descriptive Properties
UL File Number, USAE121562 
Printer friendly version Printer friendly version


New MatWeb Services

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。