SABIC Innovative Plastics VALOX EF4530 PBT (North America)
Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
| Physical Properties | Original Value | Comments |
|
| Density | 1.67 g/cc | ASTM D 792 |
| Viscosity | 480000 cP | Melt Viscosity; GE Test |
Mechanical Properties |
|
| Tensile Strength @ Break | 19000 psi | Type I, 0.2 in/min; ASTM D 638 |
| Elongation at Break | 3 % | Type I, 0.2 in/min; ASTM D 638 |
| Flexural Modulus | 1.675e+006 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Flexural Strength | 28000 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Izod Impact, Unnotched | 8 ft-lb/in | 73F; ASTM D 4812 |
| Izod Impact, Notched | 1.2 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
| Arc Resistance | Max 60 sec | Tungsten (+/- 0.125 inch); PLC Code 7; ASTM D 495 |
| Comparative Tracking Index | 175 - 250 V | (+/- 0.125 inch); PLC Code 3; UL 746A |
| Hot Wire Ignition, HWI | Min 120 sec | (+/- 0.125 inch); PLC Code 0; UL 746A |
| High Amp Arc Ignition, HAI | 30 - 60 arcs | Surface (+/- 0.125 inch); PLC Code 2; UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | Min 150 mm/min | (+/- 0.125 inch); PLC Code 4; UL 746A |
Thermal Properties |
|
| Deflection Temperature at 0.46 MPa (66 psi) | 428 °F | 0.250 inch, unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 410 °F | 0.250 inch, unannealed; ASTM D 648 |
| UL RTI, Electrical | 140 °C | UL 746B |
| UL RTI, Mechanical with Impact | 125 °C | UL 746B |
| UL RTI, Mechanical without Impact | 140 °C | UL 746B |
| Flammability, UL94 | V-0 | 0.03 in. |
| Flammability, UL94 | 7 | 0.118 in. |
Descriptive Properties | |
| UL File Number, USA | E121562 | |
|
Printer friendly version |
|