SABIC Innovative Plastics VALOX FV699 PBT (North America)
Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
Physical Properties | Original Value | Comments |
|
Density | 1.14 g/cc | Molded Foam; ASTM D 792 |
Density | 1.27 g/cc | ASTM D 792 |
Water Absorption | 0.12 % | 24 hours @ 73F; ASTM D 570 |
Water Absorption at Saturation | 0.28 % | Equilibrium, 73F; ASTM D 570 |
Linear Mold Shrinkage | 0.0035 - 0.0055 cm/cm | Flow, 0.250 inch; ASTM D 955 |
Mechanical Properties |
|
Tensile Strength @ Yield | 7200 psi | 0.250"; ASTM D 638 |
Elongation at Break | 6.9 % | 0.250"; ASTM D 638 |
Tensile Modulus | 355000 psi | 0.250"; ASTM D 638 |
Flexural Modulus | 430000 psi | 0.250"; ASTM D 790 |
Flexural Yield Strength | 11900 psi | 0.250"; ASTM D 790 |
Izod Impact, Unnotched | 19 ft-lb/in | 73F; ASTM D 4812 |
Falling Dart Impact | 14 ft-lb | 73F; GE Test |
Electrical Properties |
|
Volume Resistivity | 1.6e+016 ohm-cm | ASTM D 257 |
Surface Resistivity per Square | Min 1.1e+017 ohm | ASTM D 257 |
Dielectric Constant | 2.58 | 100 Hz; ASTM D 150 |
Dielectric Constant | 2.73 | 1 MHz; ASTM D 150 |
Dielectric Strength | 328 V/mil | in air, 250 mils; ASTM D 149 |
Dissipation Factor | 0.0024 | 100 Hz; ASTM D 150 |
Dissipation Factor | 0.0414 | 1 MHz; ASTM D 150 |
Arc Resistance | 60 - 120 sec | Tungsten (+/- 0.125 inch); PLC Code 6; ASTM D 495 |
Comparative Tracking Index | 100 - 175 V | (+/- 0.125 inch); PLC Code 4; UL 746A |
High Voltage Arc-Tracking Rate, HVTR | Min 150 mm/min | (+/- 0.125 inch); PLC Code 4; UL 746A |
Thermal Properties |
|
CTE, linear 68°F | 18 µin/in-°F | Flow, -40F to 200F; ASTM E 831 |
Specific Heat Capacity | 0.312 BTU/lb-°F | ASTM C 351 |
Deflection Temperature at 0.46 MPa (66 psi) | 240 °F | 0.250 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 226 °F | 0.250 inch, unannealed; ASTM D 648 |
UL RTI, Electrical | 75 °C | UL 746B |
UL RTI, Mechanical with Impact | 75 °C | UL 746B |
UL RTI, Mechanical without Impact | 75 °C | UL 746B |
Flammability, UL94 | V-0 | 0.154 in. |
Flammability, UL94 | 7 | 0.197 in. |
Flammability Test | 0.99 | FOAM - Flame Class Minimum Density; g/cm3 |
Oxygen Index | 29.4 % | ASTM D 2863 |
Descriptive Properties | |
Foam Weight Reduction | 10% | Mechanical Properties Reported Herein (0.250") |
Foam Weight Reduction | 10% | Impact Properties Reported Herein (0.250") |
Foam Weight Reduction | 10% | Thermal Properties Reported Herein (0.250") |
Foam Weight Reduction | 10% | Physical Properties Reported Herein (0.250") |
Foam Weight Reduction | 20% | Electrical Properties Reported Herein (0.250") |
UL File Number, USA | E121562 | |
|