SABIC Innovative Plastics VALOX K4630 PBT (North America)
Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
Physical Properties | Original Value | Comments |
|
Density | 1.5 g/cc | ASTM D 792 |
Linear Mold Shrinkage | 0.008 - 0.01 cm/cm | Flow, 0.125 inch; ASTM D 955 |
Linear Mold Shrinkage, Transverse | 0.01 - 0.012 cm/cm | 0.125 inch; ASTM D 955 |
Melt Flow | 20 g/10 min | 250C/5.0 kgf; ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Break | 14900 psi | Type I, 0.2 in/min; ASTM D 638 |
Tensile Strength @ Yield | 14500 psi | Type I, 0.2 in/min; ASTM D 638 |
Elongation at Break | 3.3 % | Type I, 0.2 in/min; ASTM D 638 |
Elongation at Yield | 3.1 % | Type I, 0.2 in/min; ASTM D 638 |
Tensile Modulus | 592000 psi | 0.2 in/min; ASTM D 638 |
Flexural Modulus | 820000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Strength | 22000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Izod Impact, Unnotched | 8.9 ft-lb/in | 73F; ASTM D 4812 |
Gardner Impact @ 23°C | 60 in-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
Izod Impact, Notched | 1 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
Arc Resistance | 120 - 180 sec | Tungsten (+/- 0.125 inch); PLC Code 5; ASTM D 495 |
Comparative Tracking Index | 175 - 250 V | (+/- 0.125 inch); PLC Code 3; UL 746A |
Hot Wire Ignition, HWI | Min 120 sec | (+/- 0.125 inch); PLC Code 0; UL 746A |
High Amp Arc Ignition, HAI | Min 120 arcs | Surface (+/- 0.125 inch); PLC Code 0; UL 746A |
High Voltage Arc-Tracking Rate, HVTR | Min 150 mm/min | (+/- 0.125 inch); PLC Code 4; UL 746A |
Thermal Properties |
|
CTE, linear 68°F | 12 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
CTE, linear 68°F, Transverse to Flow | 11 µin/in-°F | from -40F to 100F; ASTM E 831 |
Deflection Temperature at 0.46 MPa (66 psi) | 418 °F | 0.125 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 373 °F | 0.125 inch, unannealed; ASTM D 648 |
Vicat Softening Point | 415 °F | Rate B; ASTM D 1525 |
UL RTI, Electrical | 75 °C | UL 746B |
UL RTI, Mechanical with Impact | 75 °C | UL 746B |
UL RTI, Mechanical without Impact | 75 °C | UL 746B |
Flammability, UL94 | V-0 | 0.03 in. |
Flammability, UL94 | 7 | 0.118 in. |
Descriptive Properties | |
UL File Number, USA | E121562 | |
|