SABIC Innovative Plastics VALOX 412E PBT (North America)
Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
| Physical Properties | Original Value | Comments |
|
| Density | 1.45 g/cc | ASTM D 792 |
| Water Absorption | 0.06 % | 24 hours @ 73F; ASTM D 570 |
| Linear Mold Shrinkage | 0.004 - 0.006 cm/cm | Flow, 60-125 mil; ASTM D 955 |
| Linear Mold Shrinkage | 0.006 - 0.008 cm/cm | Flow, 125-180 mil; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.005 - 0.008 cm/cm | 60-125 mil; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.008 - 0.011 cm/cm | 125-180 mil; ASTM D 955 |
Mechanical Properties |
|
| Hardness, Rockwell R | 119 | ASTM D 785 |
| Tensile Strength @ Break | 14500 psi | Type I, 0.2 in/min; ASTM D 638 |
| Flexural Modulus | 750000 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Flexural Strength | 22500 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Izod Impact, Unnotched | 13 ft-lb/in | 73F; ASTM D 4812 |
| Izod Impact, Notched | 1.3 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
| Volume Resistivity | Min 1.7e+016 ohm-cm | ASTM D 257 |
| Dielectric Constant | 3.5 | 100 Hz; ASTM D 150 |
| Dielectric Constant | 3.5 | 1 MHz; ASTM D 150 |
| Dielectric Strength | 465 V/mil | in air, 125 mils; ASTM D 149 |
| Dielectric Strength | 570 V/mil | in oil, 62 mils; ASTM D 149 |
| Dissipation Factor | 0.001 | 100 Hz; ASTM D 150 |
| Dissipation Factor | 0.02 | 1 MHz; ASTM D 150 |
Thermal Properties |
|
| CTE, linear 68°F | 19 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
| CTE, linear, 212°F (100°C) | 19 µin/in-°F | Flow, 140F to 280F; ASTM E 831 |
| Deflection Temperature at 0.46 MPa (66 psi) | 412 °F | 0.250 inch, unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 395 °F | 0.250 inch, unannealed; ASTM D 648 |
|