SABIC Innovative Plastics VALOX 430 PBT (North America)
Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.
| Physical Properties | Original Value | Comments |
|
| Density | 1.52 g/cc | ASTM D 792 |
| Water Absorption | 0.05 % | 24 hours @ 73F; ASTM D 570 |
| Linear Mold Shrinkage | 0.003 - 0.005 cm/cm | Flow, 60-125 mil; ASTM D 955 |
| Linear Mold Shrinkage | 0.005 - 0.008 cm/cm | Flow, 125-180 mil; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.004 - 0.006 cm/cm | 60-125 mil; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.006 - 0.009 cm/cm | 125-180 mil; ASTM D 955 |
Mechanical Properties |
|
| Hardness, Rockwell R | 125 | ASTM D 785 |
| Tensile Strength @ Break | 16500 psi | Type I, 0.2 in/min; ASTM D 638 |
| Elongation at Break | 2 % | Type I, 0.2 in/min; ASTM D 638 |
| Flexural Modulus | 1e+006 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Flexural Strength | 25000 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Izod Impact, Unnotched | 14 ft-lb/in | 73F; ASTM D 4812 |
| Izod Impact, Notched | 2.5 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
| Arc Resistance | 120 - 180 sec | Tungsten (+/- 0.125 inch); PLC Code 5; ASTM D 495 |
| Comparative Tracking Index | 400 - 600 V | (+/- 0.125 inch); PLC Code 1; UL 746A |
| Hot Wire Ignition, HWI | Min 120 sec | (+/- 0.125 inch); PLC Code 0; UL 746A |
| High Amp Arc Ignition, HAI | 30 - 60 arcs | Surface (+/- 0.125 inch); PLC Code 2; UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | 0 - 10 mm/min | (+/- 0.125 inch); PLC Code 0; UL 746A |
Thermal Properties |
|
| Deflection Temperature at 0.46 MPa (66 psi) | 431 °F | 0.250 inch, unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 400 °F | 0.250 inch, unannealed; ASTM D 648 |
| UL RTI, Electrical | 130 °C | UL 746B |
| UL RTI, Mechanical with Impact | 130 °C | UL 746B |
| UL RTI, Mechanical without Impact | 140 °C | UL 746B |
| Flammability, UL94 | HB | 0.058 in. |
Descriptive Properties | |
| UL File Number, USA | E121562 | |
|