SABIC Innovative Plastics VALOX 771 PBT (North America)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line.

Physical PropertiesOriginal ValueComments
Density1.72 g/cc ASTM D 792
Linear Mold Shrinkage0.0065 - 0.0085 cm/cm Flow; ASTM D 955
Linear Mold Shrinkage, Transverse0.01 - 0.012 cm/cm ASTM D 955

Mechanical Properties
Tensile Strength @ Break10500 psi Type I, 0.2 in/min; ASTM D 638
Elongation at Break2.3 % Type I, 0.2 in/min; ASTM D 638
Flexural Modulus850000 psi 0.05 in/min, 2" span; ASTM D 790
Flexural Strength16000 psi 0.05 in/min, 2" span; ASTM D 790
Izod Impact, Unnotched7 ft-lb/in 73F; ASTM D 4812
Izod Impact, Notched0.8 ft-lb/in 73F; ASTM D 256

Electrical Properties
Arc Resistance180 - 240 sec Tungsten (+/- 0.125 inch); PLC Code 4; ASTM D 495
Comparative Tracking IndexMin 600 V (+/- 0.125 inch); PLC Code 0; UL 746A
Hot Wire Ignition, HWIMin 120 sec (+/- 0.125 inch); PLC Code 0; UL 746A
High Amp Arc Ignition, HAIMin 120 arcs Surface (+/- 0.125 inch); PLC Code 0; UL 746A
High Voltage Arc-Tracking Rate, HVTR0 - 10 mm/min (+/- 0.125 inch); PLC Code 0; UL 746A

Thermal Properties
Deflection Temperature at 0.46 MPa (66 psi)423 °F 0.250 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)385 °F 0.250 inch, unannealed; ASTM D 648
UL RTI, Electrical140 °C UL 746B
UL RTI, Mechanical with Impact125 °C UL 746B
UL RTI, Mechanical without Impact140 °C UL 746B
Flammability, UL94V-2 0.024 in.
Flammability, UL94V-0 0.03 in.
Flammability, UL947 0.079 in.

Descriptive Properties
UL File Number, USAE121562 
Printer friendly version Printer friendly version


Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。