MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

COMSOL CD

SABIC Innovative Plastics ULTEM 1010F Polyetherimide (Europe)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their European product line. This product is also a part of their North American product line.

Physical PropertiesOriginal ValueComments
Density1.27 g/cc ASTM D 792
Density1.27 g/cc ISO 1183
Water Absorption0.25 % 24 hours; ASTM D 570
Moisture Absorption at Equilibrium0.7 % (23 C / 50% RH) 1L; ISO 15512
Water Absorption at Saturation1.25 % 23C; ISO 62
Linear Mold Shrinkage0.005 - 0.007 cm/cm Flow; ASTM D 955
Melt Flow13 g/10 min cm3/10min; Melt Volume Rate, MVR at 340C/5.0 kg; ISO 1133

Mechanical Properties
Hardness, Rockwell M109 ISO 2039/2
Hardness, H358/30140 MPa ISO 2039/1
Tensile Strength, Ultimate85 MPa 50 mm/min; ISO 527
Tensile Strength, Ultimate90 MPa ASTM D 638
Tensile Strength, Yield105 MPa ASTM D 638
Tensile Strength, Yield105 MPa 50 mm/min; ISO 527
Elongation at Break60 % ASTM D 638
Elongation at Break60 % 50 mm/min; ISO 527
Elongation at Yield6 % 50 mm/min; ISO 527
Elongation at Yield8 % ASTM D 638
Tensile Modulus3 GPa DIN 53457
Tensile Modulus3.2 GPa 1 mm/min; ISO 527
Flexural Modulus3.3 GPa DIN 53457
Flexural Modulus3.3 GPa 2 mm/min; ISO 178
Flexural Yield Strength145 MPa DIN 53452
Flexural Yield Strength160 MPa 2 mm/min; ISO 178
Ultimate Compressive Strength140 MPa ASTM D 695
Compressive Modulus2.9 GPa DIN 53454
Shear Strength100 MPa ASTM D 732
Izod Impact, Notched0.3 J/cm 23 C; ASTM D 256
Izod Impact, Notched (ISO)5 kJ/m² 80*10*4 +23 C; ISO 180/ 1A
Izod Impact, Unnotched13 J/cm 23 C; ASTM D 4812
Izod Impact, Unnotched (ISO)NB 80*10*4 +23 C; ISO 180/ 1U
Izod Impact, Unnotched Low Temp (ISO)NB 80*10*4 -30 C; ISO 180/ 1U
Izod Impact, Notched, Low Temp (ISO)5 kJ/m² 80*10*4 -30 C; ISO 180/ 1A
Taber Abrasion, mg/1000 Cycles10 CS-17, 1 kg; GE Test

Electrical Properties
Volume Resistivity1e+015 ohm-cm IEC 60093
Surface Resistivity per SquareMin 1e+015 ohm ROA; IEC 60093
Dielectric Constant2.9 50 Hz; IEC 60250
Dielectric Constant2.9 1 MHz; IEC 60250
Dielectric Strength28 kV/mm in oil, 1.6 mm; IEC 60243-1
Dissipation Factor0.0005 50 Hz; IEC 60250
Dissipation Factor0.0025 2450 MHz; IEC 60250
Dissipation Factor0.006 1 MHz; IEC 60250
Comparative Tracking Index100 V M; IEC 60112/3rd
Comparative Tracking Index150 V IEC 60112/3rd

Thermal Properties
CTE, linear 100°C50 µm/m-°C 23C-150C, flow; ISO 11359-2
CTE, linear 100°C50 µm/m-°C 23C-150C, cross flow; ISO 11359-2
Thermal Conductivity0.21 W/m-K ISO 8302
Deflection Temperature at 0.46 MPa (66 psi)195 °C HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 0.46 MPa (66 psi)207 °C ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)190 °C HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Deflection Temperature at 1.8 MPa (264 psi)197 °C ASTM D 648
Vicat Softening Point211 °C B/50; ISO 306
Vicat Softening Point212 °C B/120; ISO 306
Vicat Softening Point215 °C A/50; ISO 306
Vicat Softening Point219 °C Rate B; ASTM D 1525
UL RTI, Electrical170 °C UL 746B
UL RTI, Mechanical with Impact170 °C UL 746B
UL RTI, Mechanical without Impact170 °C UL 746B
Flammability, UL94V-0 0.71 mm
Flammability, UL947 94-3 mm
Oxygen Index47 % ISO 4589
Glow Wire Test960 °C Passes at 3.2 mm; IEC 60695-2-1

Descriptive Properties
Ball Pressure Test, 125 C +/- 2 CPASSES IEC 60035-1
MPa; Hardness, H961/30200 DIN 53456
Printer friendly version Printer friendly version


Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。