SABIC Innovative Plastics ULTEM 2212R Polyetherimide (Europe)
Subcategory: Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their European product line. This product is also a part of their North American product line.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
| Physical Properties | Original Value | Comments |
|
| Density | 1.43 g/cc | ASTM D 792 |
| Density | 1.43 g/cc | ISO 1183 |
| Linear Mold Shrinkage | 0.003 - 0.005 cm/cm | Flow; ASTM D 955 |
Mechanical Properties |
|
| Tensile Strength, Ultimate | 75 MPa | 5 mm/min; ISO 527 |
| Elongation at Break | 8 % | 5 mm/min; ISO 527 |
| Tensile Modulus | 4.5 GPa | 1 mm/min; ISO 527 |
| Flexural Yield Strength | 135 MPa | 2 mm/min; ISO 178 |
| Compressive Modulus | 4.5 GPa | ASTM D 695 |
| Izod Impact, Unnotched (ISO) | 30 kJ/m² | 80*10*4 +23 C; ISO 180/ 1U |
Thermal Properties |
|
| Thermal Conductivity | 0.28 W/m-K | ISO 8302 |
| Deflection Temperature at 0.46 MPa (66 psi) | 202 °C | HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be |
| Deflection Temperature at 1.8 MPa (264 psi) | 189 °C | HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae |
| Vicat Softening Point | 211 °C | B/120; ISO 306 |
| Vicat Softening Point | 220 °C | Rate B; ASTM D 1525 |
| UL RTI, Electrical | 170 °C | UL 746B |
| UL RTI, Mechanical with Impact | 170 °C | UL 746B |
| UL RTI, Mechanical without Impact | 170 °C | UL 746B |
| Flammability, UL94 | V-0 | 0.41 mm |
|
Printer friendly version |

|