COMSOL CD

SABIC Innovative Plastics ULTEM 2410 Polyetherimide (Europe)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their European product line. This product is also a part of their North American product line.

Physical PropertiesOriginal ValueComments
Density1.61 g/cc ASTM D 792
Density1.61 g/cc ISO 1183
Water Absorption0.12 % 24 hours; ASTM D 570
Moisture Absorption at Equilibrium0.4 % (23 C / 50% RH) 1L; ISO 15512
Water Absorption at Saturation0.8 % 23C; ISO 62
Linear Mold Shrinkage0.001 - 0.003 cm/cm Flow; ASTM D 955
Melt Flow7 g/10 min cm3/10min; Melt Volume Rate, MVR at 360C/5.0 kg; ISO 1133

Mechanical Properties
Hardness, Rockwell M125 ISO 2039/2
Hardness, H358/30170 MPa ISO 2039/1
Tensile Strength, Ultimate180 MPa 5 mm/min; ISO 527
Tensile Strength, Yield186 MPa ASTM D 638
Elongation at Break2 % 5 mm/min; ISO 527
Elongation at Break2.5 % ASTM D 638
Tensile Modulus11.5 GPa 1 mm/min; ISO 527
Tensile Modulus11.7 GPa DIN 53457
Flexural Modulus10 GPa 2 mm/min; ISO 178
Flexural Modulus11.7 GPa DIN 53457
Flexural Strength240 MPa 2 mm/min; ISO 178
Ultimate Compressive Strength200 MPa ASTM D 695
Compressive Modulus10 GPa DIN 53454
Shear Strength103 MPa ASTM D 732
Izod Impact, Notched1.05 J/cm 23 C; ASTM D 256
Izod Impact, Unnotched4.3 J/cm 23 C; ASTM D 4812
Izod Impact, Unnotched (ISO)35 kJ/m² 80*10*4 +23 C; ISO 180/ 1U
Izod Impact, Unnotched Low Temp (ISO)35 kJ/m² 80*10*4 -30 C; ISO 180/ 1U
Charpy Impact Unnotched4 J/cm² 23C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU
Charpy Impact, Unnotched Low Temp4 J/cm² at -30C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU
Taber Abrasion, mg/1000 Cycles20 CS-17, 1 kg; GE Test

Electrical Properties
Volume Resistivity1e+015 ohm-cm IEC 60093
Surface Resistivity per SquareMin 1e+015 ohm ROA; IEC 60093
Dielectric Constant3.1 1 MHz; IEC 60250
Dielectric Constant3.5 50 Hz; IEC 60250
Dielectric Strength16 kV/mm in oil, 3.2 mm; IEC 60243-1
Dielectric Strength26 kV/mm in oil, 1.6 mm; IEC 60243-1
Dielectric Strength35 kV/mm in oil, 0.8 mm; IEC 60243-1
Dissipation Factor0.0019 1 MHz; IEC 60250
Dissipation Factor0.0025 50 Hz; IEC 60250
Comparative Tracking Index100 V M; IEC 60112/3rd
Comparative Tracking Index150 V IEC 60112/3rd

Thermal Properties
CTE, linear 100°C15 µm/m-°C 23C-150C, flow; ISO 11359-2
CTE, linear 100°C45 µm/m-°C 23C-150C, cross flow; ISO 11359-2
Thermal Conductivity0.29 W/m-K ISO 8302
Deflection Temperature at 0.46 MPa (66 psi)215 °C HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 0.46 MPa (66 psi)216 °C ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)210 °C HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Deflection Temperature at 1.8 MPa (264 psi)213 °C ASTM D 648
Vicat Softening Point217 °C B/50; ISO 306
Vicat Softening Point225 °C B/120; ISO 306
Vicat Softening Point230 °C A/50; ISO 306
Vicat Softening Point234 °C Rate B; ASTM D 1525
UL RTI, Electrical105 °C UL 746B
UL RTI, Mechanical with Impact105 °C UL 746B
UL RTI, Mechanical without Impact105 °C UL 746B
Flammability, UL94V-0 0.25 mm
Flammability, UL947 94-1.5 mm
NBS Smoke Density1 Flaming, Ds 4 min; ASTM E 662
NBS Smoke Density20 Flaming, Dmax 20 min; ASTM E 662
Oxygen Index48 % ISO 4589
Glow Wire Test960 °C Passes at 3.2 mm; IEC 60695-2-1

Descriptive Properties
Ball Pressure Test, 125 C +/- 2 CPASSES IEC 60035-1
Printer friendly version Printer friendly version


Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。