SABIC Innovative Plastics ULTEM 6200 Polyetherimide (Europe)
Subcategory: Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their European product line.
Physical Properties | Original Value | Comments |
|
Density | 1.43 g/cc | ASTM D 792 |
Water Absorption | 0.22 % | 24 hours; ASTM D 570 |
Mechanical Properties |
|
Tensile Strength, Ultimate | 145 MPa | ASTM D 638 |
Elongation at Break | 4 % | ASTM D 638 |
Tensile Modulus | 6.9 GPa | DIN 53457 |
Flexural Modulus | 6.5 GPa | DIN 53457 |
Flexural Strength | 210 MPa | DIN 53452 |
Ultimate Compressive Strength | 170 MPa | ASTM D 695 |
Shear Strength | 95 MPa | ASTM D 732 |
Izod Impact, Notched | 0.8 J/cm | 23 C; ASTM D 256 |
Izod Impact, Unnotched | 4 J/cm | 23 C; ASTM D 4812 |
Electrical Properties |
|
Volume Resistivity | 1e+015 ohm-cm | IEC 60093 |
Dielectric Strength | 23 kV/mm | in oil, 1.6 mm; IEC 60243-1 |
Thermal Properties |
|
Deflection Temperature at 0.46 MPa (66 psi) | 225 °C | ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 223 °C | ASTM D 648 |
Vicat Softening Point | 243 °C | Rate B; ASTM D 1525 |
Flammability, UL94 | V-0 | 1.5 mm |
Flammability Test | 3.2 | mm; IEC Needle Flame Test, 10 s , passes at; IEC 60695-2-2 |
NBS Smoke Density | 4 | Flaming, Ds 4 min; ASTM E 662 |
Oxygen Index | 44 % | ISO 4589 |
Descriptive Properties | |
Needle Flame Test, 3.2 mm, Burn Time s | PASSES | IEC 60695-2-2 |
|