SABIC Innovative Plastics VALOX VX5121 PBT (Europe)
Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their European product line.
| Physical Properties | Original Value | Comments |
|
| Density | 1.38 g/cc | ASTM D 792 |
| Density | 1.38 g/cc | ISO 1183 |
| Linear Mold Shrinkage | 0.003 - 0.008 cm/cm | Flow; ASTM D 955 |
| Melt Flow | 25 g/10 min | cm3/10min; Melt Volume Rate, MVR at 250C/2.16 kg; ISO 1133 |
Mechanical Properties |
|
| Hardness, H358/30 | 95 MPa | ISO 2039/1 |
| Tensile Strength, Ultimate | 90 MPa | 5 mm/min; ISO 527 |
| Elongation at Break | 1.8 % | 5 mm/min; ISO 527 |
| Tensile Modulus | 5.9 GPa | 1 mm/min; ISO 527 |
| Flexural Modulus | 5.4 GPa | 2 mm/min; ISO 178 |
| Flexural Strength | 135 MPa | 2 mm/min; ISO 178 |
| Izod Impact, Notched (ISO) | 4 kJ/m² | 80*10*4 +23 C; ISO 180/ 1A |
| Izod Impact, Unnotched (ISO) | 25 kJ/m² | 80*10*4 +23 C; ISO 180/ 1U |
| Izod Impact, Unnotched Low Temp (ISO) | 27 kJ/m² | 80*10*4 -30 C; ISO 180/ 1U |
| Izod Impact, Notched, Low Temp (ISO) | 4 kJ/m² | 80*10*4 -30 C; ISO 180/ 1A |
| Charpy Impact Unnotched | 2.7 J/cm² | 23C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU |
| Charpy Impact, Notched, Low Temp | 0.4 J/cm² | at -30C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA |
| Charpy Impact, Unnotched Low Temp | 3 J/cm² | at -30C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU |
| Charpy Impact, Notched | 0.5 J/cm² | 23C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA |
Thermal Properties |
|
| Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be |
| Deflection Temperature at 1.8 MPa (264 psi) | 170 °C | HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae |
| Vicat Softening Point | 175 °C | B/120; ISO 306 |
Descriptive Properties | |
| Ball Pressure Test, 125 C +/- 2 C | PASSES | IEC 60035-1 |
|
Printer friendly version |
|