SABIC Innovative Plastics ULTEM® CRS5112 Polyetherimide, 10% Glass Filled, Injection Grade
Subcategory: Filled/Reinforced Thermoplastic; Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Data for 3.2 mm (1/8 in) samples unless otherwise noted. Data provided by GE Plastics.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.36 g/cc | ASTM D792 |
Melt Flow | 9 g/10 min | 335°C/6.6kg; ASTM D1238 |
Mechanical Properties |
|
Tensile Strength, Ultimate | 82 MPa | ASTM D638 |
Elongation at Break | 16 % | ASTM D638 |
Flexural Modulus | 3.9 GPa | 6.4 mm sample; ASTM D790 |
Flexural Yield Strength | 152 MPa | ASTM D790 |
Izod Impact, Notched | 0.4 J/cm | 3.2 mm sample; ASTM D256 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 207 °C | 6.4 mm (0.25 in.) sample; ASTM D648 |
|