SABIC Innovative Plastics ULTEM® HTX1050F Polyetherimide, Unfilled, Injection/Extrusion Grade
Subcategory: Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Data for 3.2 mm (1/8 in) samples unless otherwise noted. Data provided by GE Plastics.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.26 g/cc | ASTM D792 |
Melt Flow | 8 g/10 min | 335°C/6.6kg; ASTM D1238 |
Mechanical Properties |
|
Tensile Strength, Ultimate | 91 MPa | ASTM D638 |
Elongation at Break | 60 % | ASTM D638 |
Flexural Modulus | 2.8 GPa | 6.4 mm sample; ASTM D790 |
Flexural Yield Strength | 134 MPa | ASTM D790 |
Izod Impact, Notched | 1.9 J/cm | 3.2 mm sample; ASTM D256 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 200 °C | 6.4 mm (0.25 in.) sample; ASTM D648 |
Processing Properties |
|
Processing Temperature | 348 - 371 °C | Suggested injection molding melt temperature |
Mold Temperature | 135 - 162 °C | |
Drying Temperature | 135 °C | |
Dry Time | 4 - 6 hour | 10 hr Max. |
|