SABIC Innovative Plastics ULTEM® HTX2001F Polyetherimide+PCE, Unfilled, Injection Grade
Subcategory: Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Data for 3.2 mm (1/8 in) samples unless otherwise noted. Data provided by GE Plastics.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.26 g/cc | ASTM D792 |
Melt Flow | 15 g/10 min | 335°C/6.6kg; ASTM D1238 |
Mechanical Properties |
|
Tensile Strength, Ultimate | 83 MPa | ASTM D638 |
Elongation at Break | 97 % | ASTM D638 |
Modulus of Elasticity | 2.7 GPa | ASTM D638 |
Flexural Modulus | 2.7 GPa | 6.4 mm sample; ASTM D790 |
Flexural Yield Strength | 120 MPa | ASTM D790 |
Izod Impact, Notched | 2.1 J/cm | 3.2 mm sample; ASTM D256 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 6.4 mm (0.25 in.) sample; ASTM D648 |
Processing Properties |
|
Processing Temperature | 321 - 348 °C | Suggested injection molding melt temperature |
Mold Temperature | 121 - 148 °C | |
Drying Temperature | 135 °C | 8 MAX. |
Dry Time | 3 - 6 hour | 8 hr Max. |
|
Printer friendly version |
|