SABIC Innovative Plastics ULTEM® 1010S PEI, Unfilled
Subcategory: Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Data provided by GE Plastics. This product grade was removed from GE's database of standard products in 1998.
Physical Properties | Original Value | Comments |
|
Density | 1.27 g/cc | ASTM D792 |
Water Absorption | 0.25 % | 24 hrs at 23°C; ASTM D570 |
Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | at 3.2 mm. |
Mechanical Properties |
|
Tensile Strength, Ultimate | 105 MPa | ASTM D638 |
Elongation at Break | 60 % | ASTM D638 |
Tensile Modulus | 2.963 GPa | ASTM D638 |
Flexural Modulus | 3.307 GPa | ASTM D790 |
Flexural Yield Strength | 152 MPa | ASTM D790 |
Izod Impact, Notched | 0.33 J/cm | 23°C (73.4°F) |
Electrical Properties |
|
Electrical Resistivity | 1e+017 ohm-cm | ASTM D257 |
Thermal Properties |
|
Deflection Temperature at 0.46 MPa (66 psi) | 207 °C | ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 197 °C | ASTM D648 |
Vicat Softening Point | 218 °C | ASTM D1525 |
|