SABIC Innovative Plastics ULTEM® 7642 PEI, Unfilled
Subcategory: Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Data provided by GE Plastics. This product grade was removed from GE's database of standard products in 1998.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Original Value | Comments |
|
Density | 1.36 g/cc | ASTM D792 |
Linear Mold Shrinkage | 0.0025 - 0.0045 cm/cm | at 3.2 mm. |
Mechanical Properties |
|
Tensile Strength, Ultimate | 152 MPa | ASTM D638 |
Elongation at Break | 2 % | ASTM D638 |
Flexural Modulus | 8.957 GPa | ASTM D790 |
Izod Impact, Notched | 0.53 J/cm | 23°C (73.4°F) |
Electrical Properties |
|
Surface Resistance | 1e+007 ohm | |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | ASTM D648 |
Processing Properties |
|
Processing Temperature | 354 - 376 °C | melt temperature |
Mold Temperature | 135 - 162 °C | |
|