Gharda Chemicals GAFONE™ 3300 PES, High Viscosity Grade

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polyethersulfone; Polymer; Thermoplastic

Close Analogs: Solvay Advanced Polymers completed its acquisition of Gharda Polymers Division in May 2006. Current product data sheets are available under the Solvay Advanced Polymers name.

Material Notes:
Unreinforced high viscosity grade for injection molding, extrusion molding, blow molding, calendering, etc.

Characteristics:

  • Very high rigidity
  • Good dielectric properties
  • High mechanical strength
  • Good dimensional stability
  • Good resistance to hydrolysis and sterilization
  • Good oxidative stability
  • Inherent flame retardance

Applications:

  • Reusable hypodermic syringes
  • Surgical instruments and components
  • Printed circuit boards
  • Circuit breaker components
  • Oil level indicators
  • Heat exchanger parts
  • Engine components
  • Household appliances
  • Filter housings
  • Sanitary and pipe fittings

Information provided by Gharda.

Physical PropertiesOriginal ValueComments
Density1.37 g/cc ISO 1183
Moisture Absorption at Equilibrium0.4 % ISO 62
Linear Mold Shrinkage0.005 cm/cm ASTM D955
Melt Flow26 - 40 g/10 min 380°C, 2.16 kg, 6 mins; ASTM D1238

Mechanical Properties
Tensile Strength at Break90 MPa ISO 527
Elongation at Break6 % ISO 527
Tensile Modulus2.8 GPa ISO 527
Flexural Modulus2.6 GPa ISO 178
Flexural Strength120 MPa ISO 178
Izod Impact, Notched (ISO)5 kJ/m² ISO 180/1A

Electrical Properties
Volume ResistivityMin 1e+016 ohm-cm IEC 93
Surface ResistanceMin 1e+014 ohm IEC 93
Dielectric Strength16 kV/mm IEC 243/1
Arc Resistance80 sec ASTM D495
Comparative Tracking Index150 V IEC 112

Thermal Properties
Maximum Service Temperature, Air185 °C Continuous use
Deflection Temperature at 1.8 MPa (264 psi)205 °C ISO 75
Glass Temperature225 °C DSC
Flammability, UL94V-0 
Oxygen Index38 % ISO 4589
Printer friendly version Printer friendly version


Free Trade Publications, Click Here!

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。