EMS-Grivory Grilon® RVZ-15H.1 Nylon 6, 15% Glass Fiber Filled, Dry As Molded

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 6; Polymer; Thermoplastic

Material Notes:
Grilon RVZ-15H.1 Black 9697 is an extrusion blow moldable, 15% glass fiber reinforced, high viscosity, heat stabilized polyamide 6 that exhibits high impact strength even at low temperatures.

Due to its very high melt strength, Grilon RVZ-15H.1 is particularly well suited for the production of large extrusion blow molded articles. It can easily be processed on conventional and 3D machines.

Grilon RVZ-15H.1 is suitable for technical articles of all kinds, especially automotive applications. Examples of possible applications include; Air ducts for turbo-chargers, Oil filler pipes, Air ducts, Fuel and oil containers and Resonators.

Information provided by EMS-Grivory

Physical PropertiesOriginal ValueComments
Density1.19 g/cc ASTM D792
Water Absorption1.23 % 24 hr immersion; ASTM D570
Water Absorption2.5 % 23°C / 50% RH; ASTM D570
Water Absorption at Saturation8 % 23°C in water; ASTM D570
Linear Mold Shrinkage0.003 cm/cm ASTM D955
Linear Mold Shrinkage, Transverse0.007 cm/cm ASTM D955

Mechanical Properties
Hardness, Shore D85 
Tensile Strength at Break90 MPa ASTM D638
Elongation at Break10 % ASTM D638
Flexural Modulus3.565 GPa ASTM D790
Flexural Strength133 MPa ASTM D790
Izod Impact, Notched3.95 ft-lb/in ASTM D256

Thermal Properties
CTE, linear 20°C120 µm/m-°C transverse; ASTM E831
CTE, linear 20°C35 µm/m-°C longitudinal; ASTM E831
Melting Point221 °C DSC
Deflection Temperature at 0.46 MPa (66 psi)220 °C ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)181 °C ASTM D648

Processing Properties
Feed Temperature100 - 160 °C Extrusion
Rear Barrel Temperature250 - 260 °C Zone 3 (Extrusion)
Middle Barrel Temperature250 - 260 °C Zone 2 (Extrusion)
Front Barrel Temperature250 - 260 °C Zone 1 (Extrusion)
Adapter Temperature240 - 250 °C Extrusion
Die Temperature446 - 482 °F Extrusion
Melt Temperature250 - 260 °C Extrusion
Mold Temperature40 - 90 °C Extrusion
Drying Temperature100 °C Vacuum Oven
Drying Temperature80 °C Dehumidifying Dryer (dew point at -40°F)
Drying Temperature80 °C Circulating Air Oven
Dry Time6 - 16 hour Circulating Air Oven
Dry Time4 - 16 hour Vacuum Oven
Dry Time4 - 16 hour Dehumidifying Dryer (dew point at -40°F)
Printer friendly version Printer friendly version


Instant Quotes for Quick Parts!Upload your 3D CAD model, select process, quantity, material, and instantly receive your unique, binding quote.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。