EMS-Grivory Grilon® FE 8023 Natural Nylon 6, Dry As Molded
Subcategory: Nylon; Nylon 6; Polymer; Thermoplastic
Material Notes: Grilon FE 8023 natural is a new heat stabilized injection molding grade based on Polyamide 6.Information provided by EMS-Grivory
Physical Properties | Original Value | Comments |
|
Density | 1.15 g/cc | ISO 1183 |
Linear Mold Shrinkage | 0.009 cm/cm | ISO 294 |
Linear Mold Shrinkage, Transverse | 0.006 cm/cm | ISO 294 |
Melt Flow | 57.5 g/10 min | 275°C / 5kg; ISO 11133 |
Mechanical Properties |
|
Tensile Strength at Break | 100 MPa | 5 mm/min; ISO 527 |
Elongation at Break | 3 % | 5 mm/min; ISO 527 |
Tensile Modulus | 4.6 GPa | 1 mm/min; ISO 527 |
Charpy Impact Unnotched | 7 J/cm² | ISO 179/1eU |
Charpy Impact, Notched, Low Temp | 0.4 J/cm² | -30°C; ISO 179/1eA |
Charpy Impact, Unnotched Low Temp | 6.5 J/cm² | -30°C; ISO 179/1eU |
Charpy Impact, Notched | 0.4 J/cm² | ISO 179/1eA |
Thermal Properties |
|
Melting Point | 220 °C | ISO 11357 |
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | ISO 75 |
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | ISO 75 |
Processing Properties |
|
Melt Temperature | 240 - 300 °C | Injection molding |
Mold Temperature | 80 - 100 °C | Injection molding |
Hold Pressure | 50 - 75 MPa | |
Back Pressure | 0.5 - 1.5 MPa | |
Screw Speed | 50 - 100 rpm | |
|
Printer friendly version |
|