EMS-Grivory Grilon® XS 1306.1 Nylon 610, Dry As Molded
Subcategory: Nylon; Nylon 610; Polymer; Thermoplastic
Material Notes: Grilon XS 1306.1 is a medium viscosity, nylon 6.10 homopolymer. It is particularly well-suited for monofilaments. Grilon XS 1306.1 exhibits excellent strength, toughness, ductility, heat stability and abrasion resistance. Grilon XS 1306.1 also offers very good resistance to a wide range of chemicals, solvents, oils and greases.Information provided by EMS-Grivory
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
| Physical Properties | Original Value | Comments |
|
| Density | 1.08 g/cc | ASTM D792 |
| Water Absorption | 0.46 % | 24 hr immersion; ASTM D570 |
Mechanical Properties |
|
| Hardness, Shore D | 81 | |
| Tensile Strength at Break | 61 MPa | ASTM D638 |
| Elongation at Break | 30 % | ASTM D638 |
| Flexural Modulus | 2.145 GPa | ASTM D790 |
| Flexural Strength | 90 MPa | ASTM D790 |
| Izod Impact, Notched | 0.8 ft-lb/in | ASTM D256 |
Thermal Properties |
|
| Melting Point | 222 °C | DSC |
| Deflection Temperature at 0.46 MPa (66 psi) | 136 °C | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 53 °C | ASTM D648 |
Processing Properties |
|
| Rear Barrel Temperature | 232 °C | Extrusion |
| Rear Barrel Temperature | 245 °C | Injection Molding |
| Middle Barrel Temperature | 232 °C | Extrusion |
| Middle Barrel Temperature | 255 °C | Injection Molding |
| Front Barrel Temperature | 227 °C | Extrusion |
| Front Barrel Temperature | 265 °C | Injection Molding |
| Nozzle Temperature | 255 °C | Injection Molding |
| Die Temperature | 450 °F | Extrusion |
| Melt Temperature | 233 °C | Extrusion |
| Melt Temperature | 265 °C | Injection Molding |
| Mold Temperature | 60 °C | Injection Molding |
|
Printer friendly version |

|