EMS-Grivory Grilon® XS 1423 Natural Nylon 6, Dry As Molded
Subcategory: Nylon; Nylon 6; Polymer; Thermoplastic
Material Notes: Grilon XS1423 Natural is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon XS1423 Natural is used typically for co-extruded fuel lines, coolant pipes in deep freezer units, vulcanization mandrels, and vacuum lines. Information provided by EMS-Grivory
| Physical Properties | Original Value | Comments |
|
| Density | 1.08 g/cc | ASTM D792 |
| Melt Flow | 18.4 g/10 min | 275°C / 5kg; ASTM D1238 |
Mechanical Properties |
|
| Tensile Strength at Break | 54.3 MPa | 50 mm/min; ASTM D638 |
| Elongation at Break | 41 % | 50 mm/min; ASTM D638 |
| Flexural Modulus | 0.348 GPa | 2 mm/min; ASTM D790 |
Processing Properties |
|
| Processing Temperature | 230 - 260 °C | Metering zone |
| Processing Temperature | 230 - 260 °C | Compression zone |
| Feed Temperature | 190 - 250 °C | |
| Nozzle Temperature | 230 - 260 °C | |
| Melt Temperature | 230 - 260 °C | Basic Machine Settings |
| Head Temperature | 230 - 260 °C | |
| Drying Temperature | Max 100 °C | Vacuum Oven |
| Drying Temperature | Max 80 °C | Desiccant Dryer (dew point at -30°C) |
| Dry Time | 4 - 12 hour | Desiccant Dryer (dew point at -30°C) |
| Dry Time | 4 - 12 hour | Vacuum Oven |
|