PolyOne Edgetek® PI-1000 Polyetherimide (PEI)
Subcategory: Polyetherimide; Polymer; Thermoplastic
Material Notes: The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.Description/Features: - PEI (Polyetherimide)
- Unfilled
- Hi-Temp
Applications: Multi-purpose Processing Method: Injection Molding Information provided by PolyOne Corporation
| Physical Properties | Original Value | Comments |
|
| Specific Gravity | 1.27 g/cc | ASTM D792 |
| Water Absorption | 0.25 % | 24 hr. Immersion, 0.125 in; ASTM D570 |
| Linear Mold Shrinkage | 0.007 - 0.009 cm/cm | ASTM D955 |
Mechanical Properties |
|
| Tensile Strength @ Yield | 15200 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
| Elongation at Break | 7 - 8 % | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
| Tensile Modulus | 430000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
| Flexural Modulus | 420000 psi | ASTM D790 |
| Flexural Strength | 22000 psi | ASTM D790 |
| Izod Impact, Notched | 1 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F(23°C); ASTM D256 |
Thermal Properties |
|
| Deflection Temperature at 1.8 MPa (264 psi) | 392 °F | Unannealed; ASTM D648 |
Processing Properties |
|
| Melt Temperature | 620 - 700 °F | Molding |
|
Printer friendly version |
|