PolyOne Geon® 1250-xx01D Vinyl Compound - Wire & Cable
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - UL Recognized 720 hr. Sunlight Resistant Jacket per UL QMTT2
- UL 60°C
- SJT
- Excellent Low Temp Impact
- Flame Retardant
Applications: Market: Processing Method: PolyOne First ChoiceDisclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications. Information provided by PolyOne Corporation.
| Physical Properties | Original Value | Comments |
|
| Specific Gravity | 1.3 g/cc | ASTM D792 |
Mechanical Properties |
|
| Hardness, Shore A | 73 | 15 sec; ASTM D2240 |
| Tensile Strength, Yield | 2200 psi | Type 4 - Flexibles, 20 in/min; ASTM D638 |
| Elongation at Break | 350 % | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Thermal Properties |
|
| Brittleness Temperature | -59.8 °F | ASTM D746 |
| Oxygen Index | 25 % | 0.075 in; ASTM D2863 |
Processing Properties |
|
| Melt Temperature | 330 - 340 °F | Extrusion |
Descriptive Properties | |
| Oven Aged - Retention of Elongation (ROE) | 80 % | 212°F (100°C), 168 hrs (7 days), 0.075 in; UL Standard |
| Oven Aged - Retention of Tensile Strength (ROT) | 90 % | 212°F (100°C), 168 hrs (7 days), 0.075 in; UL Standard |
| Product Form | Pellets/Cubes | |
|
Printer friendly version |
|