PolyOne Geon® 1351 Vinyl Compound - Flexible (FPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - Enhanced Heat Stability
- High Flow
Applications: - General Purpose
- Fence Wire Coating
Processing Method: Information provided by PolyOne Corporation.
Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.32 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore D | 63 | 15 sec; ASTM D2240 |
Tensile Strength, Ultimate | 3000 psi | 20 in/min, 100% in/in; ASTM D638 |
Tensile Strength, Ultimate | 3150 psi | 20 in/min; ASTM D638 |
Elongation at Break | 170 % | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Thermal Properties |
|
Brittleness Temperature | 32 °F | ASTM D746 |
Processing Properties |
|
Melt Temperature | 345 - 355 °F | Extrusion |
Descriptive Properties | |
Product Form | Pellets | |
|
Printer friendly version |
|