PolyOne Geon® 1604-xx27FRD Vinyl Compound - Wire & Cable
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - UL 75°C
- Matte Finish
- General Purpose Jacket Compound
- CMR
- CL2
- CL2R
- CL3R
- FPLR
- Flame Retardant
Applications: Market: Processing Method: PolyOne First ChoiceDisclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications. Information provided by PolyOne Corporation.
Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.4 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore A | 82 | 15 sec; ASTM D2240 |
Tensile Strength, Ultimate | 1950 psi | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Elongation at Break | 230 % | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Thermal Properties |
|
Brittleness Temperature | -25.6 °F | ASTM D746 |
Oxygen Index | 31 % | 0.075 in; ASTM D2863 |
Processing Properties |
|
Melt Temperature | 340 - 350 °F | Extrusion |
Descriptive Properties | |
Oven Aged - Retention of Elongation (ROE) | 100 % | 235°F (113°C), 168 hrs (7 days), 0.075 in; UL Standard |
Oven Aged - Retention of Tensile Strength (ROT) | 85 % | 235°F (113°C), 168 hrs (7 days), 0.075 in; UL Standard |
Product Form | Pellets/Cubes | |
|
Printer friendly version |
|