PolyOne Geon® 1802-xx17FRD Vinyl Compound - Wire & Cable
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - UL Recognized 720 hr. Sunlight Resistant Jacket per UL QMTT2
- PLTC
- UL 75°C
- Flame Retardant
Applications: - Power and Control Cable Jacket
Market: Processing Method: PolyOne First ChoiceDisclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications. Information provided by PolyOne Corporation.
Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.39 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore A | 88 | 15 sec; ASTM D2240 |
Tensile Strength, Yield | 3000 psi | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Elongation at Break | 300 % | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Thermal Properties |
|
Brittleness Temperature | -4 °F | ASTM D746 |
Oxygen Index | 30 % | 0.075 in; ASTM D2863 |
Processing Properties |
|
Melt Temperature | 345 - 355 °F | Extrusion |
Descriptive Properties | |
Oven Aged - Retention of Elongation (ROE) | 90 % | 212°F (100°C), 168 hrs (7 days), 0.075 in; UL Standard |
Oven Aged - Retention of Tensile Strength (ROT) | 100 % | 212°F (100°C), 168 hrs (7 days), 0.075 in; UL Standard |
Product Form | Pellets/Cubes | |
|