PolyOne Geon® 2192 Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - Transparent
- Medium Impact
- High Gloss
Applications: - FDA (Food Contact)
- Bottles
Market: Processing Method: Information provided by PolyOne Corporation.
Physical Properties | Original Value | Comments |
|
Density | 50 lb/ft³ | ASTM D1505 |
Specific Gravity | 1.34 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Rockwell R | 100 | ASTM D785 |
Hardness, Shore D | 81 | Instantaneous; ASTM D2240 |
Tensile Strength, Yield | 6400 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Tensile Modulus | 347400 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Flexural Modulus | 407 ksi | ASTM D790 |
Flexural Strength | 11400 psi | ASTM D790 |
Izod Impact, Notched | 2.1 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 154 °F | Unannealed, 0.125 in bars; ASTM D648 |
Optical Properties |
|
Transmission, Visible | 81 % | 33.0 mils, 400 nm |
Transmission, Visible | 84 % | 33.0 mils, 700 nm |
Processing Properties |
|
Melt Temperature | 390 - 415 °F | Blow Molding |
Descriptive Properties | |
Product Form | Pellets | |
|
Printer friendly version |
|