PolyOne Geon® 2710 CLR 9500 Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
The formula has a green blue tint Description/Features: - High Impact
- High Flow
- Transparent
- High Gloss
- UV Stabilized
Applications: - FDA (Food Contact)
- Hotel Amenities
- Mouthwash
- Cosmetics
Processing Method: PolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties | Original Value | Comments |
|
Density | 52 lb/ft³ | ASTM D1505 |
Specific Gravity | 1.32 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore D | 82 | Instantaneous; ASTM D2240 |
Tensile Strength, Yield | 6440 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Tensile Modulus | 341600 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Flexural Modulus | 380 ksi | ASTM D790 |
Flexural Strength | 11210 psi | ASTM D790 |
Izod Impact, Notched | 1.9 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 68 °F | Unannealed, 0.125 in bars; ASTM D648 |
Optical Properties |
|
Transmission, Visible | 69 % | 30.0 mils, 400 nm |
Transmission, Visible | 85 % | 30.0 mils, 700 nm |
Descriptive Properties | |
Product Form | Pellets | |
|
Printer friendly version |
|