PolyOne Geon® 2797 Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - Transparent
- High Gloss
- Chemical Resistant
- Medium Impact
Applications: Market: Processing Method: PolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties | Original Value | Comments |
|
Density | 50 lb/ft³ | ASTM D1505 |
Specific Gravity | 1.33 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore D | 81 | Instantaneous; ASTM D2240 |
Tensile Strength, Yield | 6650 psi | Type 1 - Rigids, 2 in/min; ASTM D638 |
Tensile Modulus | 369000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Flexural Modulus | 356 ksi | ASTM D790 |
Flexural Strength | 9870 psi | ASTM D790 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 142 °F | Unannealed, 0.125 in bars; ASTM D648 |
Optical Properties |
|
Transmission, Visible | 80 % | 20.0 mils, 400 nm |
Transmission, Visible | 90 % | 20.0 mils, 700 nm |
Processing Properties |
|
Melt Temperature | 400 - 430 °F | Blow Molding |
Descriptive Properties | |
Product Form | Pellets | |
|
Printer friendly version |
|