PolyOne Geon® 2800 IND-BL-1 Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
A high gloss transparent rigid PVC Compound designed for Industrial Blow Molding applications. This Compound is specifically formulated for large clear blow molded parts. Description/Features: Applications: Processing Method: - Extrusion - Profile, Sheet, Foam, Blow Molding
Information provided by PolyOne Corporation.
Physical Properties | Original Value | Comments |
|
Density | 48.42 lb/ft³ | ASTM D1505 |
Specific Gravity | 1.32 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore D | 82 | Instantaneous; ASTM D2240 |
Tensile Strength, Yield | 6600 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Elongation at Break | 160 % | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Flexural Modulus | 401 ksi | ASTM D790 |
Flexural Strength | 11400 psi | ASTM D790 |
Izod Impact, Notched | 14 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Processing Properties |
|
Melt Temperature | 380 - 410 °F | Blow Molding |
Descriptive Properties | |
Product Form | Pellets | |
|