PolyOne Geon® 3201-xx05D Vinyl Compound - Wire & Cable
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - UL Recognized per QMFZ2
- UL 60°C
- UL 94 HB
- Flame Retardant
Applications: - Apparatus & Cord Molding
- Plug Molding
Market: Processing Method: PolyOne First ChoiceDisclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications. Information provided by PolyOne Corporation.
Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.32 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore A | 62 | 15 sec; ASTM D2240 |
Tensile Strength, Yield | 1800 psi | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Elongation at Break | 375 % | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Thermal Properties |
|
Brittleness Temperature | -58 °F | ASTM D746 |
Flammability, UL94 | HB | All Colors; 0.059 in.; PolyOne Internal |
Processing Properties |
|
Melt Temperature | 310 - 320 °F | Molding |
Descriptive Properties | |
Product Form | Pellets/Cubes | |
|