PolyOne Geon® 3311-xx13D Vinyl Compound - Wire & Cable
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - UL Recognized per QMFZ2
- UL 75°C
- UL 94 V0
- Flame Retardant
Applications: Market: PolyOne First ChoiceDisclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications. Information provided by PolyOne Corporation.
Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.36 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore D | 68 | 15 sec; ASTM D2240 |
Tensile Strength, Yield | 4450 psi | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Elongation at Break | 180 % | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Thermal Properties |
|
Flammability, UL94 | V-0 | All Colors; 0.03 in. |
Processing Properties |
|
Melt Temperature | 360 - 380 °F | Extrusion |
Descriptive Properties | |
Product Form | Pellets/Cubes | |
|